| Sign In | Join Free | My futurenowinc.com |
|
Brand Name : KAIXIN
Model Number : KA-ALLOY no6625
Certification : ISO9001:2015
Place of Origin : China
MOQ : 30kg
Price : 38-40 USD/kg
Supply Ability : 10000KG/MONTH
Delivery Time : 15-20 DAYS
Packaging Details : Wooden Box, size as per guests request
Corrosion Resistance : Excellent
Density : 8.2 g/cm3
Elongation : Up to 40%
Formability : Good
Hardness : Up to 40 HRC
Material : Inconel Alloy
Melting Point : 1350-1400°C (2460-2550°F)
Modulus of Elasticity : 200 GPa (29 x 10 6 psi)
Tensile Strength : Up to 1,400 MPa (200,000 psi)
Thermal Conductivity : 25 W/mK (100 BTU in/hr ft² °F)
Thermal Expansion : 13.3 μm/m°C (7.3 x 10-6 in/in°F)
Type : Nickel-Chromium-Based Superalloy
Name : no6625 /Alloy 625 TIG
No6625 is a nickel-chromium-molybdenum alloy that has been specifically designed to possess high strength, corrosion resistance, and oxidation resistance. One of the key features of Inconel 625 is its ability to withstand high temperatures and withstand long-term creep under heavy loads.
No6625 has a microstructure that consists of a combination of intermetallic phases and interdiffused metal phases. These microstructural features contribute to the alloy's strength and resistance to corrosion.
One of the key microstructural features of UNS N06625 is the formation of phase precipitates. These precipitates are composed of Ni3(Nb, Al, Ti) and have a tetragonal crystal structure. The γ” phase precipitates are ordered A3 B type, meaning they have a particular arrangement of atoms.
These γ” phase precipitates are coherent with respect to the matrix, meaning they form a disk-shaped morphology and are stable at high temperatures. However, there are also some γ” phase precipitates that have a needle-like morphology and are not coherent with the matrix.
The formation of these γ” phase precipitates is important for the material's ability to recover creep properties. When subjected to long-term creep under heavy loads, the γ” phase precipitates can recover some of the alloy's strength and elongation, thereby prolonging the material's lifetime.
Overall, the combination of the microstructure and γ” phase precipitates of No6625 contribute to its exceptional performance in high-temperature and high-load environments.
| Pipe Seamless | Pipe Welded | Tube Seamless | Tube Welded | Sheet/Plate | Bar | Forging | Fitting | welding Wire |
|---|---|---|---|---|---|---|---|---|
| B444 | B705 | B444 | B704 | B443 | B446 | – | – | AWS 5.14:2018 |
No6625 W.Nr. 2.4856 ,UNS NO6625,Nickel Alloy 625,Inconel 625
Markets for No6625 include:
Product and technology applications of No6625 include:
|
|
No6625 Welding Rod Alloy 625 TIG Nickel Chromium Based Superalloy Images |